>>>Operational Example Assembly Line Method Chart.
Product line
  First Oven Second Oven Third Oven    

Rough leather Brush primer Brush first glue Brush second glue Stiking Add Pressure Check quality of shoes after 24 hours
Illustration:
1、set the temperature of first oven with 50-60℃ 5、Press up the shoe within 3 min right after sticking-step
2、set the temperature of second oven with 60-65℃ 6、 The volume of hardener added is about 3-5% of the adhesive.
3、set the temperature of third oven with 65-75℃ 7、Rubber must be rough carefully to avoid degumming
4、about 6-8 minute of line speed while the shoe go through the third oven 8、Leather and pu coating leather must be roughed heavily to avoid degumming.